How to print nylon filament
Nylon rewards a careful setup. Here is a starting point that works for many printers.
Typical starting settings
| Nozzle temperature | About 240–290 °C, depending on type (see nylon types) |
|---|---|
| Bed temperature | About 70–100 °C |
| Part cooling fan | Off or low; a little more for bridges |
| Enclosure | Strongly recommended |
| Nozzle | Hardened nozzle for CF or GF nylon |
These ranges are general guidance only. Nylon blends vary a lot between brands, so start with your filament maker's recommended settings and adjust from there, staying within the limits of your printer and hotend.
1. Start with dry filament
Many of the most common nylon print problems are caused or worsened by moisture. Many makers choose to dry nylon before printing, even when the spool is new and sealed. See drying and storing nylon.
2. Check your hotend
Some nylons need higher nozzle temperatures than PLA or PETG. Confirm that your hotend is rated for the temperature your filament maker recommends. For carbon-fiber or glass-fiber nylon, a hardened nozzle is strongly recommended because the fibers can wear brass nozzles.
3. Use an enclosure
Nylon shrinks as it cools, and drafts can make corners lift or layers separate. An enclosure is strongly recommended. It can be a printer with a built-in enclosure, a ready-made tent, or another enclosure designed for your printer. Preheat with the bed on and the door closed before you start.
4. Choose a build surface
Nylon can be tricky to stick down. Common choices include garolite (G10) sheets, or PEI with a thin layer of glue stick or a nylon-specific adhesive. Check what your build plate maker recommends, and add a brim for parts with sharp corners.
5. Keep cooling low
Too much part cooling can weaken layer bonding and increase warping. Start with the fan off or low and add a little for bridges and overhangs if needed.
6. Print from a dry box if you can
For long prints, feeding from a sealed dry box with desiccant helps limit how much moisture the filament picks up during printing.
7. Ventilation
Printing nylon at higher temperatures can release fumes and fine particles. Print in a well-ventilated area and follow the ventilation and safety guidance provided by the printer and filament manufacturer.